Products of other enterprises
Technical characteristics
- KindSilicone
Description
Conventional performance: | ||||||
test item | testing standard | unit | A | B | C | |
Outside view |
visual inspection | --- | Black/white viscous liquid | transparent liquid | Brownliquid | |
4# | 5# | |||||
viscosity | GB/T 10247-2008 | mPa·s(25ºC) | 6000±1000 | ≤50 | ≤50 | 500 |
density | GB/T 13354-92 | g/cm 3 (25ºC) | 1.20 | 0.99 | 0.99 | 0.90 |
Operation process: | |||
Test item | Unit | value | |
4# | 5# | ||
mixture ratio | weight ratio | 100 :10 | |
mixture ratio | volume ratio | 100 :12 | |
Joint part c | weight ratio | 100:10:1 | |
Mixed viscosity | mPa·s(25ºC) | 3000±500 | |
Mixture density | g/cm 3 (25ºC) | 1.10 | |
operation time | min(25ºC) | 40±15 | 90±20 |
curing time | ºC/hr | 25/24 | 25/24 |
Operation time is a quantity of cement with 100 g. |
Typical performance: | ||||
test item | testing standard | Unit | value | |
4# | 5# | |||
hardness | GB/T 531.1-2008 | Shore A | 8±3 | 6±3 |
conductivity factor | GB/T 10297-1998 | W/mK | 0.17 | |
expansion coefficient | GB/T 20673-2006 | μm/(m·ºC) | 210 | |
water absorption | GB/T 8810-2005 | (24h,25ºC)% | 0.01-0.02 | |
dielectric strength | GB/T 1693-2007 | kV/mm(25ºC) | 18 | |
Loss factor | GB/T 1693-2007 | (1MHz)(25ºC) | 0.01 | |
dielectric constant | GB/T 1693-2007 | (1MHz)(25ºC) | 2.8 | |
volume resistance | GB/T 1692-92 | (DC500V)Ω·cm | 1.2×10 15 | |
Remark : All the above data come from 25 ºC and 55% RH glue curing conditions after 7 days. |